PETG is also not resistant against toluene. A month-long contact under ambient conditions results a complete swollen/disintegrated PETG material (PDL rating 0), and an year-long exposure even causes whitening [1, p. 2660]: References Chemical Resistance of Thermoplastics; Woishnis, W. A., Ebnesajjad, S., Eds.; PDL handbook series; William Andrew: ...


2

It certainly would be possible to get an indication of some of the sources of carbon through mass spectrometry and through radiocarbon dating. For example, fossil carbon sources would have little 14C, sources predating the 20th century, e.g. older trees, would have more. Post-Atomic Age sources might have more yet, beyond that due to natural decay of 14C. ...