Radius ratio of octahedral interstitial site in BCC lithium

Problem Determine the minimum radius of an atom that will just fit into (a) the tetrahedral interstitial site in FCC nickel and (b) the octahedral interstitial site in BCC lithium. Solution (a) For ...