Questions tagged [differential-scanning-calorimetry]

This tag should be applied to questions regarding the theory and application of differential scanning calorimetry (DSC).

Filter by
Sorted by
Tagged with
0
votes
0answers
22 views

What is the Difference Between the “Degree of Conversion” and the “Degree of Cure” - If Any

I am currently investigating the degree of conversion / degree of cure of UV-curing acrylic adhesives using dynamic scanning calorimetry. A thorough google (scholar) search lets me know that the term &...
2
votes
0answers
36 views

Why would the first Tg be higher than a rescan Tg of an epoxy by DSC? [closed]

I have some small cured epoxy shafts I am cutting segments out of for checking Tg by DSC. First scan gave a Tg of 118 °C, follow on was 109 °C. Scans were repeated on a new sample of the shaft with ...
2
votes
1answer
195 views

Does alumina become transparent at high temperatures?

Consider a normal opaque alumina crucible. I've heard that they become transparent at higher temperatures and therefore, are not appropriate for high precision DSC (caloric) measurements. The reason ...
1
vote
2answers
194 views

Assigning labels and answering questions using given DSC graph

I'm currently working through past exam papers in preparation for my upcoming Inorganic Chemistry exam and I got to this question. We really haven't looked at DSC graphs, so I'm not completely sure ...
1
vote
0answers
139 views

Correctness of DSC curve for polyamid or polyester

I did a DSC on a part of an alternator car belt. We already found out that it should by a polyester or a polyamid. But then we got the following DSC curve: How is it possible that the glass ...
2
votes
1answer
279 views

DSC Metal hysteresis (melt/cryst)

So we were analyzing Polymers using DSC and calibrated the system using Indium. I expected it to be a single transition only as Indium only has 1 known crystal structure and as I never worked with DSC ...
2
votes
0answers
57 views

Is Polymorphism accompanied with an energy change?

Differential Scanning Colorimetry (DSC) is a technique used to identify Polymorphism by revealing two melting points of a pure crystalline structure. DSC shows a peak associated with the formation ...