-1
$\begingroup$

phase diagram graph explanation

At point a3, I know the ratio of the liquid phase to the solid phase, but I don't get the highlighted statement which says b3 gives the composition. I thought a3 already gave the composition? Do I need to apply another lever rule where b3 is the center? If so, where would the endpoints be?

$\endgroup$
2
$\begingroup$

The statement refers to the composition of the liquid phase, which is simply the x-value of $b_3$.

| improve this answer | |
$\endgroup$
  • 2
    $\begingroup$ To more fully flesh it out: the overall composition remains at (a2,a3,...). However, the composition of the liquid is read off the liquidus curve, so is b2, while the composition of the solid is read off the solidus curve. For this diagram there is no mutual solid solubility in the solid, so the solid is pure B. $\endgroup$ – Jon Custer Nov 22 '17 at 16:51

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.