I'm doing a study a study on voltaic cells. I've been working with them for a while and one of the questions that I've had is how does the salt bridge affect the cell. I mean, I know it allows ions to move and that it'a a basic component of the pill. But, does its' concentration affect the voltage of the cell itself? Thank you.

$\endgroup$
1
  • $\begingroup$ A n ideal salt bridge just eliminates liquid-liquid junction potential without affecting the equilibrium of the cell. A non ideal salt bridge changes the observed voltage depending on the relative mobilities of the ions in the salt bridge solution. $\endgroup$ Feb 6 '14 at 11:07
1
$\begingroup$

A cell has an internal ohmic-equivalent resistance. The salt bridge is a resistive path for the flow of ions. Ions, plus their hydration shells and possible coordination shells, have low drift velocities through a medium. The salt bridge can constrain the ion current of the cell and its material equilibrium rate. A poor salt bridge by length, diameter, concentration, and permeability will increasingly adversely affect a cell's current and voltage as discharge rate increases.

$\endgroup$
0
$\begingroup$

I don't think it affects the voltage of the cell as : E°(cell)= E°(red,cathode) - E°(red,anode) so it doesn't depend on the salt bridge !

$\endgroup$