6
$\begingroup$

I have a question about Li-ion batteries. I sometimes see the two terms - intercalated lithium and metallic lithium - used when talking about this type of batteries and I was wondering what is the difference between the two?

I understand that the intercalation means that the Li cations are transferred from one electrode to another and that is why it is called intercalated lithium (or am I wrong?). But what about metallic lithium? What does that mean?

I found this on Wikipedia:

Li-ion batteries use an intercalated lithium compound as one electrode material, compared to the metallic lithium used in a non-rechargeable lithium battery

But what makes them different? In other words, what are the differences between intercalated lithium and metallic lithium? Can anyone help me to understand this?

$\endgroup$
5
$\begingroup$

Intercalation is the addition of lithium ions into a host material without significantly changing the host's structure. In my research, I will often prepare test cells where the cathode is an intercalation material, like $\ce{CoO2}$, which can accomodate (or "intercalate") layers of lithium ions between the oxygen layers in the crystal lattice to form $\ce{LiCoO2}$. It's not that there are layers of cathode material surrounding lithium, but rather there's only 1 material, but lithium ions can move into and out of it.

$$ \ce{CoO2 + Li+ + e^- -> LiCoO2} $$

I mostly use lithium metal for the anode because it's easy to work with and has a stable potential, making it a good reference electrode:

$$ \ce{Li^+ + e^- -> Li_{(s)}} $$

In this setup we have an intercalation cathode ($\ce{LiCoO2}$), and a lithium metal anode. The major downside is that when you cycle lithium metal, it forms dendrites which can puncture the separator and short-circuit the cell, leading to catastrophic failure. To solve this problem, commercial cells use graphite anodes, which can intercalate lithium ions:

$$ \ce{C6 + Li+ + e- -> LiC6} $$

This solves the dendrite problem, but makes the battery less efficient. Since dendrite formation is only a problem with repeated cycling, non-rechargeable ("primary") batteries just use lithium metal instead. Lots of researchers have tried to solve "the dendrite problem" for decades, with little success.

The diagram below shows a lithium ion battery with an intercalation cathode on the right: the green parts are lithium, the blue parts are transition metals (Ni, Co, etc.) and the red spheres are oxygen. The anode on the left is the graphite intercalation anode, but you could replace it with a metallic lithium anode.

enter image description here

$\endgroup$
1
$\begingroup$

Intercalated in this context basically means inserted, or interposed. So an intercalated lithium-ion battery has sheets or films of material separating layers of lithium. According to this Wikipedia entry:

Separator materials in lithium ion batteries must not block the transport of lithium ions while preventing the physical contact of the anode and cathode materials, e.g. short-circuiting. In a liquid cell, this separator would be a porous glass or polymer mesh that allows ion transport via the liquid electrolyte through the pores, but keeps the electrodes from contacting and shorting. However, in a thin film battery the electrolyte is a solid, which conveniently satisfies both the ion transportation and the physical separation requirements without the need for a dedicated separator.

A lithium-metal battery is simply a conventional, non-rechargeable battery in which metallic lithium serves as the anode. There is a table of the common cathode materials used in lithium-metal batteries here.

$\endgroup$
  • $\begingroup$ Thank you for the explanation. But I can find Lithium Metal even in the context of rechargeable Li-ion batteries (see: oalib.com/references/13559284). So when they are speaking about intercalated Lithium is it the atoms and when they write Lithium-metal is it the structure (as in the second link you added: Lithium batteries are batteries that have lithium as an anode?)? And can one say that an ion is a metal or it has to be in a metallic bond to characterize it as a metal? $\endgroup$ – Physther Jan 20 '17 at 19:21
  • $\begingroup$ The separator in a lithium-ion battery is independent from the question of whether the electrode are intercalation-based or not. Even with lithium metal and a conversion material, you still need a separator. $\endgroup$ – Mark Wolfman May 5 '18 at 22:19

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.