Construct the equation for the reaction between iron(II) ions, hydrogen ions ($\ce{H+}$), and oxygen to form iron(III) ions and water.

The answer is $$\ce{4Fe^{2+}(aq) + 4H+(aq) + O2(aq)->4Fe^{3+}(aq) + 2H2O(l)}$$ Can you explain how to get this answer? Thanks.

$\endgroup$
2
$\begingroup$

Rusting of iron is an electrochemical phenomenon. A certain site on the iron object acts as an anode. $$\ce{(Fe(s) -> Fe^2+(aq) + 2e ) × 2}$$ Electrons released at this spot go to another site on the object and reduce oxygen in presence of $\ce{H+}$ ions which are either obtained from water out from acidic substances in water: $$\ce{H2O -> H+ + OH-}$$ $$\ce{CO + H2O -> H2CO3}$$ $$\ce{H2CO3 -> 2H+ + CO3^2- }$$ This site behaves as cathode and reaction is $$\ce{4H+ + O2 + 4e -> 2H2O}$$ Therefore the overall reaction is : $$\ce{2Fe(s) + O2 + 4e -> 2Fe^2+(aq) + 2H2O}$$ Now the ferrous ions are further oxidised by atmospheric oxygen to ferric ions which come out as rust in form of hydrated ferric oxides. $$\ce{Fe^2+(aq) + 2H2O + 1/2O2 -> Fe2O3 + 4H+(aq)}$$

| improve this answer | |
$\endgroup$
1
$\begingroup$

In addition to what is written by user377386, I'd like to add: $$\ce{Fe^{2+}->Fe^{3+} +e-}$$ $$\ce{4H^{+} + 4e- + O2->2H2O}$$

By multiplying the first equation by four and adding the two equations, you get the equation: $$\ce{4Fe^{2+}(aq) + 4H+(aq) + O2(aq)->4Fe^{3+}(aq) + 2H2O(l)}$$

| improve this answer | |
$\endgroup$

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.