Hello~ I am a media art artists working in Korea. Recently, create a kinetic artwork using ferrofluid. I need to create an artificial pond with a diameter of 3 meters. So I need a lot of suspension liquid.

Prototyping https://youtu.be/3o33upltO34

simulation videos https://youtu.be/NE19B_2byGA

Unfortunately, I tried my solution failed.
- case 1: Deionized water 40% / isopropyl alcohol 40% / Propylene Glycol 20% (Stains occur on the glass )
- case 2: Deionized water 60% / Coco betaine surfactants 40% ( no stain but, This seems strange movements)
- case 3: Deionized water 35% / isopropyl alcohol 35% / Coco betaine surfactants 30% (Stains the glass )
- case 4: Deionized water 60% / LES surfactants 40% ( no stain but, This seems strange movements.)
- case 5: Deionized water 60% / APG surfactants 40% ( no stain but, Decomposed into many particles)
- case 6: Windex(Glass Cleaner) 100% ( no stain but, Decomposed into many particles)

I used glass types
- pyrex glass (Small stains occur)
- tempered glass (Small stains occur)
- soda-lime glass (Big stains occur)

I was always cleaning solution into a container before adding the alcohol.

And most it had hardened over time, the ferrofluid.

$\endgroup$
1
1
$\begingroup$

There's a really good video on YouTube by Nilered/Nileblue on ferrofluids. In it he suspends magnitite with oleic acid (main component of olive oil) as a surfactant and uses Kerosene (Paraffin Oil) as a carrier.

There's a PTFE 'dry lubricant' sold under the WD-40 brand name that might be able to prevent the glass from staining as it creates a thin coat of PTFE on the glass which is highly inert. Just spray the piece of glass with the PTFE Spray and wait for it to dry (~7mins). [The PTFE spray has a myriad of other uses too, you can put it on any surface you want to have low friction, to be lubricated, an unreactive surface, dust repellant surface, etc].

This might be a way around the staining issue you are getting. Or at least point you in the right direction. Good luck!

$\endgroup$

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.