I need to 'adhese' paper to plastic, but I need the adhesive to be flammable and quick burning, but without producing any ash or too many toxic fumes.
I know this is an absurd question, but does anything like this exist?
Thanks so much
Chemistry Stack Exchange is a question and answer site for scientists, academics, teachers, and students in the field of chemistry. It only takes a minute to sign up.
Sign up to join this communityI need to 'adhese' paper to plastic, but I need the adhesive to be flammable and quick burning, but without producing any ash or too many toxic fumes.
I know this is an absurd question, but does anything like this exist?
Thanks so much
Nitrocellulose(flash paper). Using acetone or something you get a gel. Caution recommended.