7
$\begingroup$

I'm looking for a wet-etchant to remove aluminum oxide created by anodizing, but not etch the unoxidized metal (with greater than 10:1 selectivity)

I know about chromium(IV) oxide and fluorine-based etchants, but those are problematic for safety and disposal. Are there other etchants? It can be an acid or a base.

$\endgroup$
2
$\begingroup$

In Fabrication of Microstructures by Wet Etching of Anodic Aluminum Oxide Substrates Chem. Mater. 2005, 17, 4049-4052,

5% phosphoric acid is used and is selective relative to aluminum, but you need to check how it would do with respect to the other metals you mention

Finally, the AAO substrate was wet-etched in a 5 wt % H3PO4 solution at 20 °C for 8 h

| improve this answer | |
$\endgroup$
0
$\begingroup$

Alumina can be dissolved in sodium carbonate. But it would expose the bare metal to aerobic corrosion.

| improve this answer | |
$\endgroup$
  • $\begingroup$ While I do not agree that it does not attempt to answer the question, at the moment this reads more like a comment than an actual answer - could you elaborate a little more, perhaps include a link to a general procedure or outline it. $\endgroup$ – Martin - マーチン Apr 13 '16 at 5:16

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.