I am writing my bachelor thesis about alternative materials for feminine hygiene products and for testing I need to know what the viscosity is of menstruation blood. Can I use water as replacement for menstruation blood because this kind of blood exists out of a big part of water? And what is the composition of menstruation blood in percentages?

$\endgroup$
2
  • 2
    $\begingroup$ H. Larsson et al., Studies on blood viscosity during the menstrual cycle and in the postmenopausal period in healthy women, Acta Obstet.Gynecol. Scand., 1989, 68, 483-486 might be interesting to get a hand on. From the abstract, it seems that for plasma viscosity increases up to day 21 of the menstruation cycle. $\endgroup$ Mar 24, 2015 at 13:34
  • 1
    $\begingroup$ I wonder if menstrual blood viscosity correlates well with circulatory blood viscosity, since the former has to do with shed tissue from the uterine walls rather than blood exposed from a cut. $\endgroup$ Mar 24, 2015 at 15:31

1 Answer 1

12
$\begingroup$

It is difficult to give a typical value as the composition and hence the physical properties of menstrual blood varies over the course of a woman's period. This reference has a good discussion which you may find useful; you can find on p. 159:

It is fair to say that a large proportion of menses samples are considerably more viscous than blood or water - about four times as viscous as venous blood and 35 times as viscous as water.

$\endgroup$

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.