7
$\begingroup$

I know that subcritical and supercritical $\ce{CO2}$ are excellent solvents. I've seen some examples of plastics being damaged by the $\ce{CO2}$ being impregnated into the plastic at very high pressures, but in general would liquid $\ce{CO2}$ be able to dissolve plastic?

$\endgroup$
2
  • 2
    $\begingroup$ What kind of plastic? $\endgroup$
    – Dissenter
    Feb 16 '15 at 23:58
  • $\begingroup$ Good question; since it is used in commercial dry-cleaning, you know it does not attack plastics used for buttons (unless they have to be removed). Anyone in the dry-cleaning business know? $\endgroup$ Feb 17 '15 at 3:07
5
$\begingroup$

From the abstract of Solubility of Polymers and Copolymers in Supercritical $\ce{CO2}$

[…] data to temperatures of 270 °C and 3000 bar […]

Over the same range of conditions, $\ce{CO2}$ cannot dissolve polyethylene, poly(acrylic acid), poly(methyl methacrylate), poly(ethyl methacrylate), polystyrene, poly(vinyl fluoride), or poly(vinylidene fluoride) […]

$\endgroup$
1
0
$\begingroup$

Depending upon the plastic polymer Liquid $\ce{CO2}$ I believe It dissolves plastic. The chance of this are low. Here is why:

$\ce{CO2}$ solvent has many desirable properties; technically speaking it is a very ‘weak’ solvent: The polarity, dielectric constant and dipole moment are less than that of most conventional organic solvents. Consequently, high-molecular-weight polymers, proteins and polar molecules are only sparingly soluble or even insoluble in $\ce{CO2}$

Scientist have tried to make this more efficient by adding fluorine to the solvent, Unfortunately, fluorinated surfactants are not a good way to solve the problem, being both expensive and harmful to the environment. This research is ongoing, however.

$\endgroup$
0
$\begingroup$

Supercritical carbon dioxide or liquid carbon dioxide is a relatively poor solvent for polar molecules. Roughly, it is similar to pentane. If a certain plastic is soluble in pentane, probably, it may dissolve in $\ce{CO2}$.

Whenever we work with supercritical $\ce{CO2}$ (for chromatography), we usually pump a small amount of methanol along with it to increase its solvation power, otherwise most of the molecules will not dissolve in pure supercritical $\ce{CO2}$, except "fatty" molecules.

$\endgroup$

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.