I want to make composite with HDPE and wood, but when I melt it I have problem to mix them, because this polymer have high viscosity.

$\endgroup$
1
$\begingroup$
  • If you use an extruder to prepare your composite material, try to use HDPE with a melt flow index: MFI of 0.1 g/10 min.