1
$\begingroup$

What is the cathode in $\ce{NiMH}$ batteries?

I’m not sure if it is $\ce{Ni(OH)2}$ or $\ce{NiOOH}$. I’m confused because I thought that these batteries are like $\ce{NiCd}$ batteries except better (more energy density, less toxic, etc.) and use a metal hydride instead of $\ce{Cd}$ as the anode (this is all info from my textbook). So I thought the cathode in both kinds of batteries was $\ce{NiOOH}$ because that was in my textbook (it said the cathode in a $\ce{NiCd}$ battery is $\ce{NiOOH}$ and mentioned nothing about the cathode for a $\ce{NiMH}$ battery).

Here are sources I've found:

$\ce{Ni(OH)2}$ as cathode:

$\ce{NiOOH}$ as the cathode:

$\endgroup$
3
$\begingroup$

The cathode is made of $\ce{NiOOH}$ when the cell is new. This can also be written $\ce{NiO(OH)}$,where the oxidation degree of $\ce{Ni(III)}$ is more evident. The cathode is made of $\ce{Ni(OH)2}$ when the cell is discharged. Whatever the nature of the anode (cadmium, hydrogen, or any other material), the cathode is working according to the equation $$\ce{NiOOH + H2O + e^- -> Ni(OH)2 + OH^-}$$ Usually the batery is built up with $\ce{Ni(OH)2}$ and it must first be charged by electrolysis according to the reverse reaction, which is often mentioned in the publications.

$\endgroup$
1
  • $\begingroup$ Got it. Thank you so much. I forgot to consider the charged vs discharged state of these batteries $\endgroup$
    – Ibby
    Jul 1 at 20:55
3
$\begingroup$

According to Nickel Metal Hydride (NiMH): Handbook and Application Manual of Energizer Nical Metal Hydride:

The nickel-metal hydride battery chemistry is a hybrid of the proven positive electrode chemistry of the sealed nickel-cadmium battery with the energy storage features of metal alloys developed for advanced hydrogen energy storage concepts. This heritage in a positive-limited battery design results in batteries providing enhanced capacities while retaining the well-characterized electrical and physical design features of the sealed nickel-cadmium battery design.

The only difference between two kinds of batteries are nickel-metal hydride battery does not use cadmium electrode. Instead, it uses am alloy-metal hydride. The eelectrochemistry as follows:

At charge state at the negative electrode: $$\ce{Alloy + H2O + e- <=> Alloy(H) + OH-}$$ The water in the electrolyte is decomposed into hydroxyl ion and hydrogen atom, which is absorbed into the alloy.

At positive electrode: $$\ce{Ni(OH)2 + OH- <=> NiOOH + H2O + e-}$$ As evident, the charge reaction is based on the oxidation of nickel hydroxide just as it is in the nickel-cadmium couple.

At discharge state at the negative electrode: $$\ce{Alloy(H) + OH- <=> Alloy + H2O + e-}$$ The hydrogen atom is desorbed and combines with a hydroxyl ion to form water while an electron is released, which is contributing an electron to the circuit.

At positive electrode: $$\ce{NiOOH + H2O + e- <=> Ni(OH)2 + OH- }$$ As evident, nickel oxyhydroxide is reduced to its lower valence state, nickel hydroxide.

For complete review of these batteries, read here and here.

$\endgroup$
1
  • $\begingroup$ Thanks for your answer. I didn’t have the equations in my book and I suspected they would look like this but it’s nice to be sure $\endgroup$
    – Ibby
    Jul 2 at 1:02

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.