I'm trying to develop a molecule that acts as a bridge between a protein and surface of SiO2 lattice. The end that binds the protein is simple and easy but I can't figure out a way to draft up how I can get the other end to bind SiO2.

So my question is, anyone have an idea on what particular molecule or reaction I can look at that targets Silicon molecules or has a high affinity for binding specifically SiO2? It doesn't even have to be a chemical bond that links the bridge to the SiO2, it could be an electrostatic/polar interaction too.

Thank you.

$\endgroup$
1
  • 5
    $\begingroup$ You should search silane chemistry. Molecules can be easily bound to silica using functionalized triethoxysilane. $\endgroup$
    – M. Farooq
    Jun 27 '21 at 20:45
1
$\begingroup$

It is not easy to bind an organic molecule to silicium oxide. It is necessary to synthesize the Si-O bond. It cannot be done starting from $\ce{SiO2}$. A possibility is to react $\ce{CH3Cl}$ over elementary silicium at high temperature to carry out the reaction : $\ce{2 CH3Cl + Si > Si(CH3)2Cl2}$. Another approach is to make methyl sodium $\ce{NaCH3}$ react with gaseous $\ce{SiCl4}$ to produce : $\ce{SiCl4 + 3 NaCH3 -> Si(CH3)3Cl}$. These compounds can react with an alcool, like for example : $\ce{Si(CH3)3Cl + ROH -> Si(CH3)3OR + HCl}$. And here you obtain a molecule belonging to the class of the silicone. It contains the bond Si-O-C that you were looking for.

$\endgroup$
1
  • $\begingroup$ thank you friend, you knew exactly what I was looking for! $\endgroup$
    – Ahmer Imam
    Jun 29 '21 at 13:18

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.