0
$\begingroup$

I have a broken off brass needle stuck in a caste aluminum hole. (It’s the pilot mixture jet on a carburetor).

I was wondering if there was a chemical that would dissolve the brass while not reacting to the aluminium.

Previously I’ve tried:

  • Using thermal expansion and contraction to loosen it.
  • Attempting to poke it out.
  • Using an air compressor to blow it out.
$\endgroup$
1
  • 1
    $\begingroup$ Concentrated nitric acid will dissolve common brasses, but not aluminum. But, even if it works well, it would be slow going for a needle in a small hole. Good luck! $\endgroup$
    – Ed V
    Jun 19 at 0:39
2
$\begingroup$

Not likely. Ammonium hydroxide will attack brass, but at high concentrations and not very fast. And worse, I don't easily find data for aluminium in concentrated $\ce{NH4OH}$, probably because it has poor resistance.

I think you are stuck with mechanical options. Simplest is another carb or subsection. Drilling it out is obvious. Strangely enough, I have bits down to possible 0.010 " diameter but I don't know where you would buy tiny drill bits; likely you will need a few. They use collets rather than chucks to hold them , so you also need a collet or two. Sounds like more expense than a carburetor.

$\endgroup$

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.