1
$\begingroup$

Just curious, would mercury form an amalgam with gold that is already part of an alloy, i.e a gold platinum alloy?

$\endgroup$
1
0
$\begingroup$

Yes, this is a traditional method of gold purification from platinum group metals.

$\endgroup$