I need to produce paper bags. Is there any simple receipt for making paper glue so that brown (packaging) paper will stick to itself?

$\endgroup$
3
  • $\begingroup$ ...do you have access to polyvinyl alcohol and other chemical ingredients, or you just want to use around-the-house stuff? $\endgroup$ – jeremy Jul 14 '14 at 16:59
  • $\begingroup$ both recipes would be appreciated $\endgroup$ – Marian Paździoch Jul 14 '14 at 17:02
  • $\begingroup$ This looks promising for homemade $\endgroup$ – jeremy Jul 14 '14 at 17:03
2
$\begingroup$

There are a few different ways of making your own glue, here are four different versions you can try :

Simple Glue Ingredients: 1/2 cup flour 1/3 cup water

Paper Mache Glue Ingredients: 1 cup flour 1/3 cup sugar 1-1/2 cup water with 1 tsp white vinegar mixed in

Cornstarch Paste Ingredients: 1-1/2 cups cold water 2 tablespoons cornstarch 2 tablespoons corn syrup 1 teaspoon white vinegar

Simple No-Cook Flour Paste: 1 cup flour 1/2 cup water 1/8 teaspoon salt

Taken from http://www.wikihow.com/Make-Glue

$\endgroup$

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.