I need to produce paper bags. Is there any simple receipt for making paper glue so that brown (packaging) paper will stick to itself?
-
$\begingroup$ ...do you have access to polyvinyl alcohol and other chemical ingredients, or you just want to use around-the-house stuff? $\endgroup$ – jeremy Jul 14 '14 at 16:59
-
$\begingroup$ both recipes would be appreciated $\endgroup$ – Marian Paździoch Jul 14 '14 at 17:02
-
$\begingroup$ This looks promising for homemade $\endgroup$ – jeremy Jul 14 '14 at 17:03
There are a few different ways of making your own glue, here are four different versions you can try :
Simple Glue Ingredients: 1/2 cup flour 1/3 cup water
Paper Mache Glue Ingredients: 1 cup flour 1/3 cup sugar 1-1/2 cup water with 1 tsp white vinegar mixed in
Cornstarch Paste Ingredients: 1-1/2 cups cold water 2 tablespoons cornstarch 2 tablespoons corn syrup 1 teaspoon white vinegar
Simple No-Cook Flour Paste: 1 cup flour 1/2 cup water 1/8 teaspoon salt
Taken from http://www.wikihow.com/Make-Glue