If you are talking about formation of propane(alkene to alkane) , then the catalyst commonly used is Nickel along with heat. Also, Platinum or Palladium can be used instead of the above combination. The process or reaction is Hydrogenation

$\endgroup$
1
  • 1
    $\begingroup$ More precisely Catalytic hydrogenation $\endgroup$