1
$\begingroup$

Unknowing that the tubes used in the centrifuge are made of polycarbonate, I cleaned them with acetone. Following, a white smoky discolouration appeared and the tubes turned opaque. Is there any way to remove this?

$\endgroup$
  • 2
    $\begingroup$ I think it's hopeless. $\endgroup$ – Ivan Neretin Aug 13 '19 at 8:16
  • 1
    $\begingroup$ About the only way I can think of is throw out the old ones and use new ones. $\endgroup$ – Jon Custer Aug 13 '19 at 13:01
  • $\begingroup$ I agree with the comments, but maybe it does not matter much? If the tubes are completely opaque, then you need new tubes. $\endgroup$ – Ed V Aug 15 '19 at 2:10