Watts up referred to the South China Morning Post in reporting that a Tsinghua University team led by Wei Fei claimed in 2018 to have manufactured carbon nanotube fibre has tensile strength of 80 gigapascals.

Has this result been verified or reproduced independently?

The study was published in Nature and is available in ResearchGate, and a pretty nice plain language summary came out of ArsTechnica.