I'm building something out of weathering steel (A606). It is chemically formulated to rust until it becomes chemically stable and stops rusting. Its composition is: Carbon: 0.22%; Manganese: 1.25%; Sulphur: 0.04% and Copper: 0.2% (minimum).

I want to accelerate the "weathering" process rather than wait for Mother Nature to do it. What chemicals should I use?

$\endgroup$
2
  • $\begingroup$ Now that's tricky. Chemicals might form a subtly different kind of rust which never becomes stable, but just continues until it eats your steel all through. $\endgroup$ Jul 12 '19 at 14:52
  • $\begingroup$ I'd ask the manufacturer. You're surely not their first customer who wants to sell a product in it's final optics. $\endgroup$
    – Karl
    Jul 12 '19 at 17:10
5
$\begingroup$

To accelerate "weathering" , give it more weather - spray it with water each day . You could add a little salt ( NaCl) initially but then let the water spray remove it over time. The steel also has some P in it and a bit of Cr ( like 0.1 % ) . The Mn is also to improve strength as A 606 is "higher" strength steel ( higher than ordinary hot rolled ). It doesn't exactly "stop" rusting ; it builds a somewhat protective layer of rust. In most environments this works well . It does not work on a seacoast or in an industrial environment. Another situation that may be a problem is above concrete or light color stone , as some red rust will slowly run off the steel over the years ( leaving drip marks on the concrete)

$\endgroup$

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.