Why is it that oxidizers (specifically $\ce{KClO3}$) are at risk of causing a fire when they come into contact with the rubber stopper used to contain them in their container, but can be slowly heated if they do not contact the rubber stopper?

Essentially, why is it that oxidizers are incompatible with rubber?

$\endgroup$
1
  • $\begingroup$ Note that an oxidiser is not combustible, it is a supporter of combustion. You need both a combustible material and a supporter if you want fire, heat is not a magical creator of fire. I'm not sure as to what the exact reaction is (oxidation of rubber) $\endgroup$ Sep 7 '12 at 6:49
4
$\begingroup$

A lot of rubbers possess C=C double bonds. Alkenes are very easily oxidized by KMnO4 or KClO3, therefore in the case where you're not aware of the chemical nature of the rubber, it's best not to expose it to strong oxidizers.

$\endgroup$
0
$\begingroup$

$\ce{KClO3}$ and $\ce{KMnO4}$ are special kind of oxidizers, that donate oxygen very, very easy. Mixtures of this oxidizers with some reducers can self-combust on friction. Rubber stopper on regular friction produce fine powder of rubber and oxidize.

The reason for it is a special property of this oxidizers, that give out oxygen of surprisingly low heating.

$\endgroup$

Your Answer

By clicking “Post Your Answer”, you agree to our terms of service, privacy policy and cookie policy

Not the answer you're looking for? Browse other questions tagged or ask your own question.